Balage P, Lopez J, Bonamis G, Hönninger C, Manek-Hönninger I. 2023. Crack-free high-aspect ratio holes in glasses by top–down percussion drilling with infrared femtosecond laser GHz-bursts. Int. J. Extrem. Manuf. 5 015102.
Citation: Balage P, Lopez J, Bonamis G, Hönninger C, Manek-Hönninger I. 2023. Crack-free high-aspect ratio holes in glasses by top–down percussion drilling with infrared femtosecond laser GHz-bursts. Int. J. Extrem. Manuf. 015102.

Crack-free high-aspect ratio holes in glasses by top–down percussion drilling with infrared femtosecond laser GHz-bursts


doi: 10.1088/2631-7990/acaa14
More Information
  • Received Date: 2022-04-11
  • Accepted Date: 2022-12-07
  • Rev Recd Date: 2022-07-07
  • Publish Date: 2023-01-30
  • We report novel results on top-down percussion drilling in different glasses with femtosecond laser GHz-bursts. Thanks to this particular regime of light–matter interaction, combining non-linear absorption and thermal cumulative effects, we obtained crack-free holes of aspect ratios exceeding 30 in sodalime and 70 in fused silica. The results are discussed in terms of inner wall morphology, aspect ratio and drilling speed.

  • 加载中
通讯作者: 陈斌, bchen63@163.com
  • 1. 

    沈阳化工大学材料科学与工程学院 沈阳 110142

  1. 本站搜索
  2. 百度学术搜索
  3. 万方数据库搜索
  4. CNKI搜索

Figures(1)

Article Metrics

Article views(297) PDF Downloads(49) Citation(0)

Crack-free high-aspect ratio holes in glasses by top–down percussion drilling with infrared femtosecond laser GHz-bursts

doi: 10.1088/2631-7990/acaa14
  • 1 Université de Bordeaux-CNRS-CEA, CELIA UMR 5107, 33405 Talence, France;
  • 2 Amplitude, Cité de la Photonique, 11 Avenue de Canteranne, 33600 Pessac, France

Abstract: 

We report novel results on top-down percussion drilling in different glasses with femtosecond laser GHz-bursts. Thanks to this particular regime of light–matter interaction, combining non-linear absorption and thermal cumulative effects, we obtained crack-free holes of aspect ratios exceeding 30 in sodalime and 70 in fused silica. The results are discussed in terms of inner wall morphology, aspect ratio and drilling speed.